Français Quote

In the field

Lithium batteries above 35 °C

Every cell datasheet, ours included, quotes cycles and capacity at 25 °C. Nobody in Benin installs a battery at 25 °C. That gap is not a laboratory detail: it is the first reason a pack ages faster than its datasheet promises.

In this article
  1. What heat does, mechanically
  2. Why LFP holds up better here
  3. The six decisions that change
  4. The threshold that really matters: charging cold
  5. How to tell whether your pack is suffering
  6. What we measure, and what we do not promise

What heat does, mechanically

A lithium cell ages along two paths. The first is cycling: each charge and each discharge damages the materials a little. The second is calendar ageing: the cell degrades simply because time passes, even sitting on a shelf.

Heat accelerates the second, and that is the part people forget. The parasitic reactions inside the cell — the growth of the interface layer on the anode, above all — track temperature. The hotter it is, the faster they go, and they consume available lithium irreversibly.

In practice, a pack sitting at 40 °C loses capacity having done nothing. And a pack working at 40 °C also heats itself through its own losses, so it is in fact running hotter than the air around it.

We publish no coefficient of the "half the cycles at 45 °C" kind, because we have not made those measurements and the figure depends on chemistry, current and charge window. What we can state is the direction of the effect, and it is always the same.

Why LFP holds up better here

This is the main reason we push LFP for fixed installations in Benin, and not only for its cycle life.

LFP has a more stable crystal structure than NMC and a higher thermal runaway temperature. On a fault — an internal short, an overcharge — it reacts less violently: it releases heat and gas where an NMC can catch fire. For a pack sitting in a plant room next to an inverter, that difference in behaviour outweighs all the others.

It also tolerates running warm day after day, which is exactly the regime of a solar kit under a metal roof.

The six decisions that change

Here is what we do differently from a temperate-climate installation, and these are not theoretical precautions.

  • The room before the pack. A shaded, ventilated pack lasts longer than a bigger pack under a metal roof. It is the cheapest decision in the whole installation, and it is the one people take last.
  • Never against a wall facing south or west, and never in a closed cupboard. A wall heated all afternoon gives its heat back at night, which is to say while the pack is discharging.
  • Air around the cells. A prismatic pack is built with a gap between cells and an air path above. Clamping cells mechanically is necessary; stopping them from breathing is not.
  • No fan by reflex. A fan in a dusty room becomes a dust pump, and dust insulates. If the room air is already at 38 °C, the fan blows 38 °C air.
  • Charge a little lower. Stopping the charge somewhat below maximum reduces the stress on the cell, and it is the only stress you can relax for free. You lose a little rated capacity and you gain years.
  • Choose a BMS with a temperature probe, and set it. Many cheap BMS have a probe but no active threshold: the probe then only displays a number.

The threshold that really matters: charging cold

Paradoxically, in an article about heat, the most dangerous threshold is a low one. Charging a lithium cell below 0 °C plates metallic lithium on the anode, irreversibly, and that can end in an internal short.

In Benin that threshold is never met outdoors. But it is met in two cases: a pack shipped in an aircraft hold, and a pack installed in a cold room. If either applies to you, the BMS must block charging below 0 °C, and not all of them do.

Conversely, discharging cold does not damage the cell: it only reduces the capacity available, temporarily. A battery that seems weak at dawn is not necessarily worn out.

How to tell whether your pack is suffering

Heat cannot be seen, it has to be measured. Three readings are enough, and they take a multimeter and a little method.

  • Real capacity, once a year. Charge fully, discharge at a known power, time it. Compare with the test report delivered with the pack. A slow loss is normal; ten per cent in a year on an LFP pack is not.
  • The spread between cells, at end of charge. That is where it speaks loudest: with the pack full, voltages should sit within a few tens of millivolts. A cell that always rises first is a cell starting to drop out.
  • The pack temperature at the end of the day, not in the morning. Put a hand on it after a discharge: if it is clearly warmer than the room air, internal losses are high, and that is often the sign of a connection that resists.

Write those readings down somewhere. A single value says nothing; it is the drift that speaks, and drift only shows against a history.

What we measure, and what we do not promise

Every pack we assemble leaves with a test report: measured capacity, each cell’s voltage, internal resistance. That is the starting point, and it lets you measure drift later.

We do not quote a number of years. An identical pack, at two customers, will have two very different lives depending on the room, the daily depth of discharge and the quality of balancing. What we can do is tell you what matters, in order, and hand you what you need to follow your pack’s condition.

If you describe where the pack will sit — indoors or under a shelter, ventilated or not, exposed or shaded — we will take it into account in the sizing and in the choice of chemistry.

Also worth reading

  • Maintaining and storing a lithium battery

    What a long outage does to a pack, the self-discharge arithmetic over six months, and the maintenance routine that fits in fifteen minutes a quarter.

  • Lead or LFP: the real ten-year cost

    Why a lead-acid bank costs more than an LFP pack over ten years, worked out in cycles and delivered energy rather than in currency.

All notes

Quote

Your request

The fields marked optional really are. Fill in what you know.

No prices online: every requirement differs, so every quote is priced on its own.

My quote request